Szczegóły Produktu:
|
| rodzaj wiązania: | Wzmocniony grafitem | Pozorna porowatość: | 5% |
|---|---|---|---|
| Zawartość MgO: | 78% | Gęstość nasypowa: | 3,05 g/cm3 |
| Zimna siła kruszenia: | 52 MPa | Refraktorowość pod obciążeniem: | 1690 r |
| Stała zawartość węgla: | 12% | ||
| Podkreślić: | C12 Blast Furnace Hearth,Graphite Enhanced Brick,High Density Hearth Unit |
||
For blast furnace hearth duty in a blast furnace, these C12 bricks combine 78% MgO with 12% carbon and a graphite enhanced matrix that resists spalling during hot metal production. Carbon content is held at 12% because that is the level where thermal conductivity, slag wetting and oxidation loss stay in balance for hot metal production. Apparent porosity of 5% keeps liquid slag from reaching the brick interior, while a cold crushing strength of 52 MPa supports the mechanical